Production of submicron silk particles by milling
Date
2013
Authors
Kazemimostaghim, Mehdi
Rajkhowa, Rangam
Tsuzuki, Takuya
Wang, Xungai
Journal Title
Journal ISSN
Volume Title
Publisher
Elsevier BV
Abstract
Bead milling was used to produce nano silk particles from silk fibres. Silk fibres were first milled to volume median particle size d(0.5) of 7. μm using an attritor mill. It was followed by bead milling to prepare submicron particles. Several processing
Description
Keywords
Keywords: Attritor mill; Bead milling; Median particle size; Milling parameters; Milling speed; Processing parameters; Silk powders; Sub-micron particles; Particle size; Particle size analysis; Silk; Spray drying; Milling (machining); alkali; nanoparticle; silk; ar Bead milling; Particle size; Silk powder; Spray drying