Investigating the effect of salt and acid impurities in supercritical CO₂ as relevant to the corrosion of carbon capture and storage pipelines

dc.contributor.authorSim, S.en
dc.contributor.authorCole, I. S.en
dc.contributor.authorBocher, F.en
dc.contributor.authorCorrigan, P.en
dc.contributor.authorGamage, R. P.en
dc.contributor.authorUkwattage, N.en
dc.contributor.authorBirbilis, N.en
dc.date.accessioned2026-06-11T08:41:03Z
dc.date.available2026-06-11T08:41:03Z
dc.date.issued2013en
dc.description.abstractA series of corrosion exposure tests were performed in a supercritical CO2 environment used to represent the potential conditions for carbon capture and storage (CCS) pipelines. Impurities from various CO2 capture processes are potentially present, which segregate to the aqueous phase, hence combining with any free water present in the pipeline. Herein, salt (NaNO3, Na2SO4, NaCl) and acid (HNO3) impurities were added, along with 10g of water, to an autoclave at 7.6MPa and 50°C (supercritical CO2) for a 7 day steel specimen exposure. The tests conducted in supercritical CO2 were also compared with aqueous tests in atmospheric conditions. Weight loss and optical profilometry revealed that corrosion rates for all samples are significant, along with the potential for localised attack. The corrosion mechanism differs for each solution tested. The work herein contributes to a holistic appraisal of understanding the corrosion of CO2 pipelines.en
dc.description.sponsorshipS.S. is supported by an MGS scholarship from Monash University . Financial support from the DRET (via the Energy Pipelines CRC) is also gratefully acknowledged.en
dc.description.statusPeer-revieweden
dc.format.extent8en
dc.identifier.issn1750-5836en
dc.identifier.otherORCID:/0000-0001-6582-1457/work/217149603en
dc.identifier.scopus84880389308en
dc.identifier.urihttps://hdl.handle.net/1885/733810488
dc.language.isoenen
dc.sourceInternational Journal of Greenhouse Gas Controlen
dc.subjectCCSen
dc.subjectCorrosionen
dc.subjectPipelineen
dc.subjectSupercriticalen
dc.titleInvestigating the effect of salt and acid impurities in supercritical CO₂ as relevant to the corrosion of carbon capture and storage pipelinesen
dc.typeJournal articleen
dspace.entity.typePublicationen
local.bibliographicCitation.lastpage541en
local.bibliographicCitation.startpage534en
local.contributor.affiliationSim, S.; Monash Universityen
local.contributor.affiliationCole, I. S.; CSIROen
local.contributor.affiliationBocher, F.; Southwest Research Instituteen
local.contributor.affiliationCorrigan, P.; CSIROen
local.contributor.affiliationGamage, R. P.; Monash Universityen
local.contributor.affiliationUkwattage, N.; Monash Universityen
local.contributor.affiliationBirbilis, N.; Department of Electronic Materials Engineering, Research School of Physics, ANU College of Science and Medicine, The Australian National Universityen
local.identifier.citationvolume17en
local.identifier.doi10.1016/j.ijggc.2013.06.013en
local.identifier.purea52308aa-3e5b-45fe-b878-d71acd2efe5aen
local.identifier.urlhttps://www.scopus.com/pages/publications/84880389308en
local.type.statusPublisheden