Kazemimostaghim, MehdiRajkhowa, RangamTsuzuki, TakuyaWang, Xungai2015-12-130032-5910http://hdl.handle.net/1885/77536Bead milling was used to produce nano silk particles from silk fibres. Silk fibres were first milled to volume median particle size d(0.5) of 7. μm using an attritor mill. It was followed by bead milling to prepare submicron particles. Several processingKeywords: Attritor mill; Bead milling; Median particle size; Milling parameters; Milling speed; Processing parameters; Silk powders; Sub-micron particles; Particle size; Particle size analysis; Silk; Spray drying; Milling (machining); alkali; nanoparticle; silk; ar Bead milling; Particle size; Silk powder; Spray dryingProduction of submicron silk particles by milling201310.1016/j.powtec.2013.03.0042016-02-24